Refine
Document Type
- Journal article (18)
- Book chapter (2)
Language
- English (20) (remove)
Is part of the Bibliography
- yes (20)
Institute
- Texoversum (20)
Publisher
- Elsevier (4)
- MDPI (3)
- dfv Mediengruppe (3)
- dfv media group (3)
- Deutscher Fachverlag (2)
- ACS (1)
- IBP, Internat. Business Press Publ. (1)
- RSC (1)
- SAGE Publications Ltd (1)
- Springer (1)
Cleanable bag filter : comparisons of different testing methods of ageing of filter materials
(2019)
Cleanable bag filters are used to separate dust and other airborne particulate systems. Due to typical process conditions, they are subject to thermal, chemical and mechanical stress during use. The main objective of the IGF project no. 18307 "Investigation of the chemical and thermal degradation of cleanable filter media and improvement of their resistance by surface modification", was the development of a valid test method which can reproduce degradation caused by high temperatures and aggressive chemical atmospheres in a practice-oriented but time-saving manner. Within the IGF project, 2 accelerated ageing methods were applied, both of which have the decisive advantage of investigating damage in the gas phase. Many resistances of filter materials are otherwise carried out by immersing the materials in a mostly liquid damage medium at a defined temperature. These resistances are difficult to transfer ageing in the gas phase.
Nanocoatings based on sol–gel coatings are presented as suitable tool to modify materials based on polymers. The main focus is set onto textiles as the most common polymer materials. It presents which types of functionalization can be reached by modified sol–gel processes. Also a suitable categorization of functions is given and set into relation to common applications. A special focus is set on the functional properties, antimicrobial, UV protective, and flame retardant. The concept of bifunctional coatings is discussed and especially the combination of water-repellent and antistatic is presented.
In the IGF project No. 19617 N, nitrogen and phosphorous substituted alkoxysilanes were prepared and their ability to inhibit fire growth and spread for fabrics was explored. To this end, a series of flame retardants were synthesized using different strategies including click chemistry and nucleophilic substitution of commercial organophosphorus compounds with amino-based trialkoxysilanes and/or cyanuric chloride. The new halogen-free and aldehyde-free flame retardants were applied to different fabrics such as cotton (CO), polyethylene terephthalate (PET), polyamide (PA) and their blends using the well-known pad-dry-cure technique and sol-gel method. The flame-retarding efficiencies were evaluated by EN ISO 15025 test methods (protective clothing-protection against heat and flame method of test for limited flame spread). Good flame retardancy of the hybrid organic-inorganic materials was achieved with the addition of as small amount as 3-5 wt.% for cotton fabrics. Moreover, the water solubility and the washing resistance could be controlled through the functional groups attached to the phosphor atom or through the optimization of the curing temperature. Overall, the research project demonstrated that N-P-silanes are very good permanent flame retardants for textiles.
Several ionic liquids are excellent solvents for cellulose. Starting from that finishing of PET fabrics with cellulose dissolved in ionic liquids like 1-ethyl 3-methyl imidazolium acetate, diethylphosphate and chloride, or the chloride of butyl-methyl imidazolium has been investigated. Finishing has been carried out from solutions of different concentrations, using microcrystalline cellulose or cotton and by employing different cross-linkers. Viscosity of solutions has been investigated for different ionic liquids,concentrations, cellulose sources, linkers and temperatures. Since ionic liquids exhibit no vapor pressure,simple pad-dry-cure processes are excluded. Before drying the ionic liquid has to be removed by a rinsing step. Accordingly rinsing with fresh ionic liquid followed by water or the direct rinsing with waterhave been tested. The amount of cellulose deposited has been investigated by gravimetry, zinc chlorideiodine test as well as reactive dyeing. Results concerning wettability, water up-take, surface resistance,wear-resistance or washing stability are presented.
The sol-gel approach offers a new class of flame retardants with a high potential for textile applications. Pure inorganic sol-gel systems do, however, typically not provide an effect sufficient for a sel-fextinguishing behavior on its own. We therefore employed compounds with nitrogen and phosphorous containing groups. Especially the combination of compounds with both elements, using the synergism, is promising for the aim to find well-applicable, environmental friendly, halogen-free flame retardants. In our approach, the sol-gel network ensured on the one hand the link to the textile as nonflammable binder. On the other hand, the sol-gel-based networks modified with functional groups containing nitrogen groups provided flame retardancy. In this way, a flame retardant finishing for textiles could be obtained by simple finishing techniques as, e.g., padding. Besides a characterization with various flame tests (e.g., according to EN ISO 15025 e protective clothing), we used a combination of cone calorimetry, thermogravimetry coupled with infrared spectroscopy analysis and scanning electron microscopy to analyze the mechanism of flame retardancy. Thus, we could show that the main mechanism is based on the formation of a protection layer. This work provides a model system for sol-gel-based flame retardants and has the potential to show the principle feasibility of the sol-gel approach in flame retardancy of textiles. It therefore lays the groundwork for tailoring sol-gel layers from newly synthesized sol-gel precursors containing nitrogen and phosphorous groups.
Three established test methods employed for evaluating the abrasion or wear resistance of textile materials were compared to gain deeper insight into the specific damaging mechanisms to better understand a possible comparability of the results of the different tests. The knowledge of these mechanisms is necessary for a systematic development of finishing agents improving the wear resistance of textiles. Martindale, Schopper, and Einlehner tests were used to analyze two different fabrics made of natural (cotton) or synthetic (polyethylene terephthalate) fibers, respectively. Samples were investigated by digital microscopy and scanning electron microscopy to visualize the damage. Damage symptoms are compared and discussed with respect to differences in the damaging mechanisms.
Indium tin oxide (ITO) particle coatings are known for high transparency in the visible, good conductive properties and near-infrared absorption. These properties depend on ITO particle's stiochiometric composition, defects and size. Here we present a method to gradually change ITO particle's optical properties by a simple and controlled laser irradiation process. The defined irradiation process and controlled energy dose input allows one to engineer the absorption and transsmission of coatings made from these particles. We investigate the role of the surrounding solvent, influence of laser fluence and the specific energy dose targeting modification of the ITO particle's morphology and chemistry by stepwise laser irradiation in a free liquid jet. TEM, SEM, EDX, XPS, XRD and Raman are used to elucidate the structural, morphological and chemical changes of the laser-induced ITO particles. On the basis of these results the observed modification of the optical properties is tentatively attributed to chemical changes, e.g. laser-induced defects or partial reduction.
The wet chemical deposition of solution processed transparent conducting oxides (TCO) provides an alternative low cost and economical deposition technique to realize large-areas of conducting films. Since the price for the most common TCO Indium Tin Oxide rises enormously, Aluminum Zinc Oxide (AZO) as alternative TCO reaches more and more interest. The optoelectronical properties of nanoparticle coatings strongly depend beneath the porosity of the coating on the shape and size of the used particles. By using bigger or rod-shaped particles it is possible to minimize the amount of grain boundaries resulting in an improvement of the electrical properties, whereas particles bigger than 100 nm should not be used if highly transparent coatings are necessary as these big particles scatter the visible light and lower the transmittance of the coatings. In this work we present a simple method to synthesize AZO particles with different shape and size, but comparable electronical properties. We use a simple, well reproducible polyol method for synthesis and influence the shape and size of the particles by adding different amounts of water to the precursor solution. We can show that the addition of aluminum as dopant strongly hinders the crystal growth but the addition of water counteracts this, so that both, spherical and rod-shaped particles can be obtained.
The requirements for textiles differ greatly depending on the area of application, whereby it often does not remain with only one required functionality. For example, in the field of functional clothing or protective clothing/PPE, it is necessary to protect the textile’s wearers from UV radiation. At the same time, self-cleaning effects offer certain advantages in that field. In addition, an antimicrobial effect in functional clothing can reduce the formation of unpleasant odors, and in PPE – especially in the healthcare sector – can contribute to the interruption of the chain of infection. One way to achieve these 3 desired functions in just one finishing step is to immobilize titanium dioxide (TiO2). However, TiO2 is viewed critically for application in the textile sector due to a REACH listing. Another disadvantage is that it only takes effect under UV radiation and is therefore not suitable for indoor use. Alternatively, photocatalysts such as doped zinc oxides (ZnO) can be used, which also exhibit catalytic activity through activation by visible light, which can lead to the killing of microorganisms and the degradation of organic soiling.
Flame-retardant finishing of cotton fabrics using DOPO functionalized alkoxy- and amido alkoxysilane
(2023)
In the present study, DOPO-based alkoxysilane (DOPO-ETES) and amido alkoxysilane (DOPO-AmdPTES) were synthesized by one-step and without by-products as halogen-free flame retardants. The flame retardants were applied on cotton fabric utilizing sol–gel method and pad-dry-cure finishing process. The flame retardancy, the thermal stability and the combustion ehaviour of treated cotton were evaluated by surface and bottom edge ignition flame test (according to EN ISO 15025), thermogravimetric analysis (TGA) and micro-scale combustion calorimeter (MCC). Unlike CO/DOPO-ETES sample, cotton treated with DOPO-AmdPTES nanosols exhibits self-extinguishing ehaviour with high char residue, an improvement of the LOI value and a significant reduction of the PHRR, HRC and THR compared to pristine cotton. Cotton finished with DOPO-AmdPTES reveals a semi-durability after ten laundering cycles keeping the flame-retardant properties unchanged. According to the results obtained from TGA-FTIR, Py-GC/MS and XPS, the major activity of flame retardant occurs in the condensed phase via catalytic induced char formation as physical barrier along with the activity in the gas phase derived mainly from the dilution effect. The early degradation of CO/DOPO-AmdPTES compared to CO/DOPO-ETES, triggered by the cleavage of the weak bond between P and C=O, as the DFT study indicated, provides the beneficial effect of this flame retardant on the fire resistance of cellulose.