The hard template method for the preparation of monodisperse mesoporous silica microspheres (MPSMs) has been established in recent years. In this process, in situ-generated silica nanoparticles (SNPs) enter the porous organic template and control the size and pore parameters of the final MPSMs. Here, the sizes of the deposited SNPs are determined by the hydrolysis and condensation rates of different alkoxysilanes in a base catalyzed sol–gel process. Thus, tetramethyl orthosilicate (TMOS), tetraethyl orthosilicate (TEOS), tetrapropyl orthosilicate (TPOS) and tetrabutyl orthosilicate (TBOS) were sol–gel processed in the presence of amino-functionalized poly (glycidyl methacrylate-co-ethylene glycol dimethacrylate) (p(GMA-co-EDMA)) templates. The size of the final MPSMs covers a broad range of 0.5–7.3 µm and a median pore size distribution from 4.0 to 24.9 nm. Moreover, the specific surface area can be adjusted between 271 and 637 m2 g−1. Also, the properties and morphology of the MPSMs differ according to the SNPs. Furthermore, the combination of different alkoxysilanes allows the individual design of the morphology and pore parameters of the silica particles. Selected MPSMs were packed into columns and successfully applied as stationary phases in high-performance liquid chromatography (HPLC) in the separation of various water-soluble vitamins.
Sol-gel-controlled size and morphology of mesoporous silica microspheres using hard templates
(2023)
Mesoporous silica microspheres (MPSMs) represent a promising material as a stationary phase for HPLC separations. The use of hard templates provides a preparation strategy for producing such monodisperse silica microspheres. Here, 15 MPSMs were systematically synthesized by varying the sol–gel reaction parameters of water-to-precursor ratio and ammonia concentration in the presence of a porous p(GMA-co-EDMA) polymeric hard template. Changing the sol–gel process factors resulted in a wide range of MPSMs with varying particle sizes from smaller than one to several micrometers. The application of response surface methodology allowed to derive quantitative predictive models based on the process factor effects on particle size, pore size, pore volume, and specific surface area of the MPSMs. A narrow size distribution of the silica particles was maintained over the entire experimental space. Two larger-scale batches of MPSMs were prepared, and the particles were functionalized with trimethoxy(octadecyl) silane for the application as stationary phase in reversed-phases liquid chromatography. The separation of proteins and amino acids was successfully accomplished, and the effect of the pore properties of the silica particles on separation was demonstrated.
Mesoporous silica microspheres (MPSMs) find broad application as separation materials in high liquid chromatography (HPLC). A promising preparation strategy uses p(GMA-co-EDMA) as hard templates to control the pore properties and a narrow size distribution of the MPMs. Here six hard templates were prepared which differ in their porosity and surface functionalization. This was achieved by altering the ratio of GMA to EDMA and by adjusting the proportion of monomer and porogen in the polymerization process. The various amounts of GMA incorporated into the polymer network of P1-6 lead to different numbers of tetraethylene pentamine in the p(GMA-co-EDMA) template. This was established by a partial least squares regression (PLS-R) model, based on FTIR spectra of the templates. Deposition of silica nanoparticles (SNP) into the template under Stoeber conditions and subsequent removal of the polymer by calcination result in MPSM1-6. The size of the SNPs and their incorporation depends on the pore parameters of the template and degree of TEPA functionalization. Moreover, the incorporated SNPs construct the silica network and control the pore parameters of the MPSMs. Functionalization of the MPSMs with trimethoxy (octadecyl) silane allows their use as a stationary phase for the separation of biomolecules. The pore characteristics and the functionalization of the template determine the pore structure of the silica particles and, consequently, their separation properties.
High-performance liquid chromatography is one of the most important analytical tools for the identification and separation of substances. The efficiency of this method is largely determined by the stationary phase of the columns. Although monodisperse mesoporous silica microspheres (MPSM) represent a commonly used material as stationary phase their tailored preparation remains challenging. Here we report on the synthesis of four MPSMs via the hard template method. Silica nanoparticles (SNPs) which form the silica network of the final MPSMs were generated in situ from tetraethyl orthosilicate (TEOS) in the presence of (3-aminopropyl) triethoxysilane (APTES) functionalized p(GMA-co-EDMA) as hard template. Methanol, ethanol, 2-propanol, and 1-butanol were applied as solvents to control the size of the SNPs in the hybrid beads (HB). After calcination, MPSMs with different sizes, morphology and pore properties were obtained and characterized by scanning electron microscopy, nitrogen adsorption and desorption measurements, thermogravimetric analysis, solid state NMR and DRIFT IR spectroscopy. Interestingly, the 29Si NMR spectra of the HBs show T and Q group species which suggests that there is no covalent linkage between the SNPs and the template. The MPSMs were functionalized with trimethoxy (octadecyl) silane and used as stationary phases in reversed-phase chromatography to separate a mixture of eleven different amino acids. The separation characteristics of the MPSMs strongly depend on their morphology and pore properties which are controlled by the solvent during the preparation of the MPSMs. Overall, the separation behavior of the best phases is comparable with those of commercially available columns. The phases even achieve faster separation of the amino acids without loss of quality.
This study introduces a straightforward approach to construct three-dimensional (3D) surface-enhanced Raman spectroscopy (SERS) substrates using chemically modified silica particles as microcarriers and by attaching metal nanoparticles (NPs) onto their surfaces. Tollens’ reagent and sputtering techniques are utilized to prepare the SERS substrates from mercapto-functionalized silica particles. Treatment with Tollens’ reagent generates a variety of silver NPs, ranging from approximately 10 to 400 nm, while sputtering with gold (Au) yields uniformly distributed NPs with an island-like morphology. Both substrates display wide plasmon resonances in the scattering spectra, making them effective for SERS in the visible spectral range, with enhancement factors (ratio of the analyte’s intensity at the hotspot compared to that on the substrate in the absence of metal nanoparticles) of up to 25. These 3D substrates have a significant advantage over traditional SERS substrates because their active surface area is not limited to a 2D surface but offers a much greater active surface due to the 3D arrangement of the NPs. This feature may enable achieving much higher SERS intensity from within streaming liquids or inside cells/tissues.